Copper foil arrives from the drum in a state you cannot laminate. The treatment process is what converts it into foil that will bond to a dielectric and survive board processing.
Foil definitions
Most of the naming in this area describes which side of the foil the adhesion treatment went on, and how rough that side ends up.
- DSTF (drum side treated foil) — the adhesion treatment is applied to the shiny drum side
- RTF (reverse treated foil) — the same thing under a different name
- LP — low profile foil, tooth between 5.1 and 9.9 microns
- VLP-X — very low profile foil, tooth below 5 microns
- e-VLP / HVLP — ultra low profile foils
- STD HTE — standard shiny copper, with the adhesion treatment applied to the matte side
Where each one is used
LP, VLP-X and e-VLP-X foils go into the applications where conductor loss at frequency is what limits the design:
- Telecom infrastructure and mobile multilayer boards
- Storage and switching hardware
- 5G mobile
- 77 GHz radar
- IoT devices
Standard HTE foil remains the sensible choice for automotive and industrial boards, where the frequencies involved do not justify paying for a smoother foil.
Reverse treated foil
In reverse treated foils, it is the smooth face of the electrodeposited copper that gets treated. The treatment layers are thin coatings that do two jobs at once: they improve how well the base foil adheres to the dielectric, and they add corrosion resistance, roughening the glossy side in the process.
When panels are built, that treated side is the one laminated to the dielectric. Because the treated drum side ends up rougher than the other face, adhesion to the dielectric is better than it would be with ordinary ED copper — which is the main reason to specify it.
There is a second benefit on the other face. The matte side needs no mechanical or chemical preparation before photoresist goes on; it is already rough enough to hold laminate resist properly.
Surface profile
Foil profile is a trade-off, and it is worth being explicit about which side of it your design sits on. A rougher tooth gives better mechanical adhesion and more margin in lamination. A smoother tooth gives lower conductor loss, which is what matters once signals get fast enough for the skin effect to push current into the outer surface of the trace. Below a few gigahertz the rough foil is usually the better engineering answer. Above it, the loss budget generally decides.
If you are not sure which side of that line your stackup falls on, send it over with the target frequency and we will come back with a recommendation.